The National Technical Information Service acquires, indexes, abstracts, and archives the largest collection of U.S. government-sponsored technical reports in existence. The NTRL offers online, free and open access to these authenticated government technical reports. Technical reports and documents in its repository may be available online for free either from the issuing federal agency, the U.S. Government Publishing Office’s Federal Digital System website, or through search engines.




Details
Actions:

Diallyl Phthalate Prepolymer Characterization and Testing in Fiberglass Filled Molding Compounds.


DE83009352

Publication Date 1983
Personal Author Whitaker, R. B.; Schneider, R. E.; Schumacher, R. J.
Page Count 21
Abstract A program was undertaken to identify an acceptable alternative to Dapon 35, an o-diallyl phthalate (DAP) prepolymer no longer available. Three o-DAP prepolymers from the Osaka Soda Company and four laboratory-scale prepolymers from Bendix-Kansas city were characterized and evaluated in DAP-fiberglass molding compounds. Gel permeation chromatography results for the Osaka prepolymers showed all three to be very close to one another in molecular weights (mw) and mw distributions, but slightly lower in both than Dapon 35. They are also slightly higher in monomer content. All three processed readily into DAP-fiberglass molding compounds and passed required physical property tests. One Osaka prepolymer was compounded into both asbestos and Orlon-DAP compounds on a production scale. Both compounds have passed all certification tests. The Bendix prepolymers were deliberately varied in mw and mw distribution and higher in monomer content than Dapon 35. Processing difficulties were encountered with both the lowest and highest molecular weight compounds, and the lowest molecular weight compound failed a number of physical property tests. The two intermediate molecular weight compounds processed readily and passed property tests. Guidelines were established for acceptable o-DAP prepolymers: (1) weight average mw (relative to polystyrene standards): 30,000 to 150,000; (2) mw distribution: 3.0 to less than or equal to 18.0; and (3) DAP monomer content: 1.0 to less than or equal to 6.0%. 5 figures, 6 tables. (ERA citation 08:024019)
Keywords
  • Molding materials
  • Fiberglass
  • Asbestos
  • Polymers
  • Evaluation
  • Phthalic acid esters
  • Chromatography
  • Molecular weight
  • Physical properties
  • Monomers
  • Phthalic acid/(diallyl-ester)
  • ERDA/360301
Source Agency
  • Technical Information Center Oak Ridge Tennessee
NTIS Subject Category
  • 71O - Plastics
  • 99F - Physical & Theoretical Chemistry
Corporate Authors Monsanto Research Corp., Miamisburg, OH. Mound.; Department of Energy, Washington, DC.
Document Type Technical Report
NTIS Issue Number 198318
Contract Number
  • AC04-76DP00053
Diallyl Phthalate Prepolymer Characterization and Testing in Fiberglass Filled Molding Compounds.
Diallyl Phthalate Prepolymer Characterization and Testing in Fiberglass Filled Molding Compounds.
DE83009352

  • Molding materials
  • Fiberglass
  • Asbestos
  • Polymers
  • Evaluation
  • Phthalic acid esters
  • Chromatography
  • Molecular weight
  • Physical properties
  • Monomers
  • Phthalic acid/(diallyl-ester)
  • ERDA/360301
  • Technical Information Center Oak Ridge Tennessee
  • 71O - Plastics
  • 99F - Physical & Theoretical Chemistry
  • AC04-76DP00053
Loading